反应器筒节焊缝开裂断口分析
Fracture Analysis on Weld Cracking of Reactor Shell Course
浏览(18) 下载(0)
- DOI:
- 作者:
- 张 鹏1 ,时培玉2
Zhang Peng1 , Shi Peiyu2
- 作者单位:
- (1.广东石化有限责任公司,广东 揭阳 515200;2.中国石油大庆石化公司,黑龙江 大庆 163714)
(1.Guangdong Petrochemical Co., Ltd., Jieyang 515200, China; 2.PetroChina Daqing Petrochemical Company, Daqing 163714, China)
- 关键词:
- 14Cr1MoR(H);复合板;加氢反应器;焊缝开裂;断口分析;脆性断裂
14Cr1MoR (H); Clad Plate; Hydrogenation Reactor; Weld Cracking; Fracture Analysis; Brittle Fracture
- 摘要:
- 某炼化一体化项目加氢反应器筒节采用 14Cr1MoR(H)+S32168 不锈钢复合板制造,筒节在焊后二次辊压矫形工序时发生纵缝整体开裂。通过宏观断口形貌观察、扫描电镜微观断口表征等手段对失效试样开展了系统检测,得出了焊缝断裂机理与失效诱因,可为铬钼+不锈钢复合板压力容器筒节焊接与成型矫形工艺优化提供参考。The shell section of a hydrogenation reactor in an integrated refining and petrochemical project was manufactured from14Cr1MoR (H)+S32168 stainless steel clad plate. Full-length cracking of the longitudinal weld occurred in the shell section duringthe post-weld secondary roll straightening process. Systematic examinations were conducted on the failed specimens via macroscop⁃ic fracture morphology observation and microscopic fracture characterization by scanning electron microscopy (SEM). The fracturemechanism of the weld joint and the failure-inducing factors were clarified. The results can provide a reference for optimizing thewelding and forming-straightening processes of pressure vessel shell sections made of Cr-Mo/stainless steel clad plates.